Laser structuring textures and micro-structures surfaces with precision - improving adhesion, wettability or functional surface properties. It’s programmable, repeatable and contactless.
How it works
A controlled beam creates defined micro-patterns on the surface. Structuring is repeatable and programmable across geometries. Used to prepare surfaces for downstream joining or coating. Parameters matched to material and target pattern at the LAC.
Where it applies
Surface texturing and micro-structuring for battery and general-industry components where surface function - adhesion, wettability, coating grip - matters.
General industry
Beyond electrode texturing, laser structuring is used to improve coating and adhesive adhesion (surface texturing ahead of painting or bonding), create controlled hydrophobic or anti-glare surface finishes, and pattern cooling or fluid-channel geometries directly into components. It also supports functional surface marking and micro-texturing for medical, optical and general industrial parts - wherever a surface needs a defined, repeatable micro-topography rather than a random finish.
How it compares
| Laser Structuring | Mechanical Abrasion | Chemical Etch/Anodise | |
|---|---|---|---|
| Feature control | High - programmable, micro/nano-scale patterns | Low - random roughness | Medium - needs masking |
| Repeatability | High | Moderate, operator-dependent | High, if controlled |
| Selectivity | Yes - can target specific areas, maskless | No | Partial (masking) |
| Throughput | Lower - pattern is scanned point-by-point | High | Medium |
| Equipment cost | Very high | Low | Low-medium |
Benefits
Precise, programmable micro- and nano-scale patterns without masks or contact · improves adhesion, wettability (hydrophobic/hydrophilic control), or friction properties on the exact area that needs it · fully automatable, no chemicals involved · minimal waste.
Limitations
Slower throughput on large areas - not suited to bulk roughening · equipment cost is the highest of the three technologies (ultrashort-pulse lasers) · line-of-sight only · quality control needs specialized metrology (profilometry, microscopy), adding inspection cost.
Safety & standards
Same Class 4 laser precautions as welding/cleaning. Structuring often ablates the base material itself, so metal-fume extraction is particularly important. Covered by the same core standards (ISO 11553, IEC 60825).
Technical Parameters
- Laser-induced surface patterns (LIPSS) typically range from ~100 nm to 10 µm in period, tunable by wavelength and pulse regime. Peer-reviewed
- Nanosecond-laser texturing of aluminum raised adhesive-joint shear strength up to +348% versus untreated surface, with contact angle dropping from 65° to 24°. Peer-reviewed
- Laser-treated steel-CFRP joints showed a +299% increase in shear strength versus untreated surfaces in the same class of study. Peer-reviewed
- Femtosecond texturing of copper current collectors has been shown to improve active-material contact and cycling performance in Li-ion cells - a directly battery-relevant structuring application. Peer-reviewed
Where this fits.
Frequently asked questions
What surfaces can you structure?
Metals used in battery and general-industry manufacturing; parameters are matched to material and target pattern.
Is the pattern repeatable?
Yes - it's programmable and repeatable across parts.
What is structuring used for?
Improving adhesion and wettability, and preparing surfaces for joining or coating.